I may go back in there some time and stuff that cell.
I'd love to find one of the several thirties sets that has chrome accents.
On the Firestone I did, not only was the veneer delaminating but the plywood top was, too. The veneer has to have a completely solid and smooth base with no imperfections or they'll telegraph through to the surface. I had to make a new plywood top for mine. If your set has several different planks on top, it's possible the joint between them could cause trouble eventually if not right away. The joint could possibly have glue forced into it and clamped tightly and then the top block-sanded smooth.
__________________
Reece