Originally Posted by jr_tech View Post
If the bonding material on a particular tube is a type of polyester resin (I believe that some were ... PPG 5252 or something like that), methylene chloride will do the job. Very nasty, however.

jr
Dow Chemical's formula is in Patent 3007833:

33 parts by weight diglycidyl etherr of bisphenol A, 67 parts diglycidyl ether of polyoxypropylene glycol having a molecular weight of 400 and 5.5 parts of monoethanolamine and 1 part of diethylenetriamine.

What that means, I dunno. The patent is for the use of a Saran wrap band around the tube and safety plate while filling the gap with the above mix.

US Patent 3265234 from Union Carbide lists a number of other chemicals that were used to bond the safety plates - about 4 or 5 formulations are compared.

I guess not all CRT's used the same bonding materials....


Cheers,
__________________
Brian
USN RET 22YRS (Avionics/Cal)
CET-Consumer Repair and Avionics ('88)
"Capacitor Cosmetologist since '79"

When fuses go to work, they quit!
Reply With Quote