Quote:
Originally Posted by jeyurkon View Post
Have you ever seen a cataract or similar form with 184? I'd expect it to last nearly forever.
Yes, I have observed partial de-lamination on some tubes using 184.... sort of looked like "worm tracks" in the material.

Quote:
Originally Posted by jeyurkon View Post
Dow 184 is nearly ideal for the purpose, but would break the bank for a large CRT.
I see that Amazon has the material listed, wonder how many 21" crts could be bonded with an 3.9kg "kit" for $336 ?